Ballistic Laboratory report available to current customers and new contacts under NDA


Refitted Panel information - Panel had been previously shot with 11 rounds of 5.56 x 45 mm SS109 and subsequently repaired. The ballistic report shows test shots after the repair : Defeated Velocity of 5.56 x 45 mm 946 (m/s) ,& Defeated Velocity of 30-06 SP 799(m/s) after second use.

 
 
 